Rear triangle.. lots going on but nothing you have not seen before if you have been following this diary of a frame fool. It all goes great until the brass.... I just cant read it. the temps are high, the color different and flux just dont tell me much... It goes fluid way before the brass is ready to flow. Silver/silver flux is easier to see.. It goes grey when the temperature is right and ready... Aaarrggg.. brass.... weird material when used with steel. Keep in mind that this is my own
"A-ha" moment to arrive at.. not yet though. The more I work with it the better. I think I am working too cool, so akin to the dynamic of silver that laying the heat on is counter to what I expect...










Moving on.. Here are some build pics along with the result.. sorry for the slop.